3dprinting:troubleshooting:stringing [11/04/2026 14:27] – created - external edit 127.0.0.13dprinting:troubleshooting:stringing [11/15/2026 23:39] (current) – added article Jon
Line 8: Line 8:
  
 Change one setting at a time and save the test result with the material profile. Change one setting at a time and save the test result with the material profile.
 +
 +====== Eliminating PLA Stringing in Bambu Studio ======
 +
 +===== 1. Dry the Filament =====
 +Moisture boiling inside the hotend creates steam pressure that forces PLA out during travel moves.
 +* **Action:** Dry PLA at **50°C–55°C for 4–6 hours** before tuning slicer settings.
 +* **Storage:** Keep spools in sealed dry boxes or an AMS with fresh desiccant.
 +
 +===== 2. Lower Nozzle Temperature =====
 +* **Location:** //Filament Settings > Filament > Print temperature//
 +* **Action:** Drop temperature in **5°C increments** (e.g., `220°C` -> `210°C` -> `205°C`).
 +* **Tool:** Run **Calibration > Temperature** in the top toolbar to find the optimal temp.
 +
 +===== 3. Tune Retraction (Direct Drive) =====
 +* **Location:** //Filament Settings > Setting Overrides//
 +* **Retraction Length:** `0.8 mm` to `1.2 mm` (Do not exceed `2.0 mm` to avoid heat creep).
 +* **Retraction Speed:** `30 mm/s` to `45 mm/s`.
 +* **Z-Hop:** Test `0.2 mm` or disable (`0 mm`) if oozing occurs during vertical lifts.
 +* **Tool:** Run **Calibration > Retraction Test** to verify.
 +
 +===== 4. Adjust Travel & Wall Routing =====
 +* **Location:** //Process > Quality (Advanced Mode)//
 +* **Avoid Crossing Walls:** **Enabled** (routes travel moves inside the part rather than across open gaps).
 +* **Wipe While Retracting:** **Enabled** (//Printer Settings > Extruder//).
 +* **Travel Speed:** Keep high (`400–500 mm/s`) to snap molten strands cleanly.
 +
 +===== Quick Diagnostic Table =====
 +^ Symptom ^ Likely Cause ^ Fix ^
 +
 +| Fine cobweb hairs | Wet filament or high temp | Dry spool at 55°C; lower temp 5–10°C |
 +| Thick branch-like blobs | Low retraction or dirty nozzle | Increase retraction to `1.0–1.2 mm`; clean nozzle tip |
 +| Stringing on small spires | Heat buildup / slow cooling | Increase cooling fan or slow down small perimeters |
  